MEMSnet Home: MEMS-Talk: Sputtering Ag on Si
Sputtering Ag on Si
2003-03-03
Dimitris Niarchos
2003-03-04
Bill Moffat
Sputtering Ag on Si
Bill Moffat
2003-03-04
Dimitris,
         Get the standard 22 degree slope back angle.  Then plasma clean with a
gentle Oxygen descum and or argon plasma surface roughness modification to
promote Si/Ag adhesion.  I have a number of technical papers on lift off and a
few production inputs on plasma treatment.  Contact me directly for more
information.  Bill Moffat

-----Original Message-----
From: Dimitris Niarchos [mailto:[email protected]]
Sent: Monday, March 03, 2003 7:36 AM
To: [email protected]
Subject: [mems-talk] Sputtering Ag on Si


Does anyone know  a good way to deposit Ag on Si - good adhesion - for
further lift-off process?


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering