sputtering of TiO2
2003-03-05
Mr Christian DRUON
2003-03-05
Swaroop Kaza
2003-03-06
Stefan Wiechmann
2003-03-06
Stefan Wiechmann
2003-03-07
Swaroop Kaza
2003-03-14
Brent Garber
sputtering of TiO2
Mr Christian DRUON
2003-03-05
Dear all,

Does anyone know a tried and tested sputtering process for the deposition of
high quality thin-film insulating titanium dioxide layers (i.e. titania,
TiO2) on pre-metallized substrates (e.g. Pt/SiO2/Si?). We are looking to
deposit thin films ( about 1000A) having a high dielectric constant (80-100)
and a good insulating behaviour (i.e. very low leakage currents). In
addition, can anyone suggest a suitable metal underlayer which gives good
crystallization of the TiO2.

Yours sincerely,


Christian DRUON
IEMN (Institut d' Electronique, de Microelectronique et de Nanotechnologies)
Departement DHS
Cite scientifique
Avenue Poincare, BP 69
59652 Villeneuve d' Ascq Cedex, FRANCE
Tel: 03.20.19.79.62
Fax:03.20.19.78.80
email: [email protected]
http://www.iemn.univ-lille1.fr



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing