dear all,
can you suggest a good organic material, depositable or spinnable at low
temperature, to be used as a protection mask for long KOH etching process?
...... it should be lifted-off or etched easily in a chemistry which do
not affect SiN layers.
thank you for any help you can provide

carlo


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing