MEMSnet Home: MEMS-Talk: RIE Etching of Ni
RIE Etching of Ni
2003-03-08
[email protected]
RIE Etching of Ni
[email protected]
2003-03-08
Greetings,

Is there a chemistry for RIE dry etching Ni?
I only need to go through 200A and then I hit a W layer I etch with SF6.

Thank You

Brent Garber

--------------------------------------------------------------------
mail2web - Check your email from the web at
http://mail2web.com/ .