MEMSnet Home: MEMS-Talk: seeking services: DRIE of glass, quartz, etc.
seeking services: DRIE of glass, quartz, etc.
2003-03-07
John Chiaverini
2003-03-10
Darden Hood
2003-03-12
[email protected]
seeking services: DRIE of glass, quartz, etc.
Darden Hood
2003-03-10
John, we don't do etching but we do do ESEM to video for QA.  If interesting
let me know.  Demos at http://www.videoem.com/videoem/demovideo.asp



Darden Hood
MicroAnalytica, LLC
4989 SW 74 Court
Miami, Florida 33155
[email protected]


----- Original Message -----
From: John Chiaverini 
To: 
Sent: Friday, March 07, 2003 12:35 PM
Subject: [mems-talk] seeking services: DRIE of glass, quartz, etc.


I'm seeking a company or fab that can do deep etching (say 20 um or more)
with vertical sidewalls into/through any of the following materials:

sapphire
glass/SiO2
quartz
aluminum nitride
alumina
diamond

These will be small wafer batches.  Any info would be useful, and you can
contact me directly.


John Chiaverini
NIST Boulder, Time and Frequency Division
Ion Storage Group, Quantum Computation Project
[email protected]
(303) 497-4364


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
University Wafer
Tanner EDA by Mentor Graphics