Kim, GunWoo
2003-03-10
Michael Yakimov
Piranha cleaning on the GaAs wafer
Michael Yakimov
2003-03-10
depending on Piranha concentration, you may expect etch rate >10
micron/minute..
for diluted solution, like H2SO4:H202(30%):H2O=1:8:80 the etch rate is ~0.8
micron/minute..
        Mike

> -----Original Message-----
> From: Kim, GunWoo [SMTP:[email protected]]
> Sent: Friday, March 07, 2003 14:45
> To:   [email protected]
> Subject:      [mems-talk] Piranha cleaning on the GaAs wafer
>
> Dear all,
> Have you experienced to use a Piranha cleaning step with GaAs wafer?
> I want to know how much attack (surface roughening or etc) will be on
> the GaAs wafer after the Piranha cleaning step.
> Please, anyone would you let me know any information about that?
> Thank you very much
>
> Gunwoo Kim
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering