Re: anodic glass-glass
2003-03-11
Gabriel, Markus
Re: anodic glass-glass
Gabriel, Markus
2003-03-11
Ziggy,

check you substrate parameters first:
1. do you use Bosilicate Glass (you need it for Anodic Bonding)?
2. what is the surface quality (TTV, bow, warpage, microroughness) of your
substrates?
3. surface quality of the deposited Si (roughness)?

bonding parameters suggestion:
450 °C, >1000V,
might help, if you have the chance to contact the Si layer with the anode

We can run some samples  for you (without a charge).

Markus.


SUSS MicroTec
Business Field MEMS
Markus Gabriel
Schleissheimer Str. 90
85748 Garching
Germany
Fon     +49 89 32007 - 313
Fax     +49 89 32007 - 390
email   [email protected]
http://www.suss.com/mems


Date: Fri, 7 Mar 2003 13:15:20 -0600 (CST)
From: Zigurts Majumdar 
Subject: [mems-talk] anodic glass-glass
To: [email protected]
Message-ID:
        
Content-Type: TEXT/PLAIN; charset=US-ASCII


Hi,
        Does anyone have a good protocol for bonding thick pieces of
glass, about 2 to 5 mm thick? I've tried using an intermediate layer of Si
with ~ 15kV, but it didn't work.

-Ziggy



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group