Deposition of Au into a microchannel
Roger Shile
2003-03-11
Due to the low pressure and lack of gas phase scattering, evaporation tends
to be directional and result in poor sidewall coverage.

Sputtering the Au, should give you better sidewall coverage, particularly at
higher pressures.

Roger Shile

----- Original Message -----
From: 
To: 
Sent: Monday, March 10, 2003 3:44 PM
Subject: [mems-talk] Deposition of Au into a microchannel


>
> Hi all,
>
> I am trying to deposit Au layer on the surface of a microchannel, both the
> walls and the bottom.  However, by evaporation the gold only deposits at
the
> bottom surface;  the walls of the channel are not covered.  I am wondering
if
> someone has experience solving this problem.
>
> Thanks alot!
>
> Zhiyu
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Harrick Plasma, Inc.
MEMStaff Inc.