Questions on Polyimide
Sang (Kevin) Kim
2003-03-11
Patrick, that depends on the type and the brand of polyimide you use. This
information is found in the manufactures process sheet. I use archchemical
polyimides.
http://www.archmicro.com/products/dtlStress.asp

Kevin

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Patrick Carlberg
Sent: Tuesday, March 11, 2003 6:01 AM
To: [email protected]
Subject: [mems-talk] Questions on Polyimide

Dear all,

Does anyone know the approximate thickness of Polyimide on Si spun at
3000rpm or the etching rate in O2-plasma.

Sincerely
Patrick Carlberg


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering
MEMS Technology Review