Patrick,
        Question 1 depends upon the type and viscosity of the Polymide.
Question 2depends upon the hardbake temperature of the Polymide and the type of
Plasma system.  For example in a microwave high power resist stripper like the
YES 108 you can remove about 8 microns of hard baked Polymide in about 5 minutes
in a barrel plasma unit 13.54 M/Hz think many hours.  If you have more specific
details let me know and I will give you more specific answers.  Bill Moffat

-----Original Message-----
From: Patrick Carlberg [mailto:[email protected]]
Sent: Tuesday, March 11, 2003 3:01 AM
To: [email protected]
Subject: [mems-talk] Questions on Polyimide


Dear all,

Does anyone know the approximate thickness of Polyimide on Si spun at
3000rpm or the etching rate in O2-plasma.

Sincerely
Patrick Carlberg


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation
MEMStaff Inc.