MEMSnet Home: MEMS-Talk: Selective etching of InGaAs over InP
Selective etching of InGaAs over InP
2003-03-12
Fabio Altomare
Selective etching of InGaAs over InP
Fabio Altomare
2003-03-12
Dear all,
 I have an heterostructure with InP and In_{0.53}Ga_{0.47}As and I'm
looking for a recipe to etch the InGaAs and leave as much of the InP as
possible.
Can any of you suggest a simple recipe for wet etching? And do you have
any idea of the etching rate for the two compound? And how about any
dependence on the crystallographic direction?
Thank you very much for all your help
Fabio



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
MEMS Technology Review
University Wafer