A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Piezoresistors
Etching of SiN
2003-03-13
Patrick Carlberg
Piezoresistors
2003-03-13
krishna
2003-03-17
mahdi bagheri
2003-03-18
krishna
reference material
2003-03-18
Frederick Balagot
2003-03-17
beaton@npphotonics (Bill Eaton)
2003-03-13
Hong Wu
2003-03-13
Roger Shile
2003-03-13
[email protected]
2003-03-13
Michael D Martin
2003-03-13
[email protected]
Piezoresistors
krishna
2003-03-13
Dear Members,

we have fabricated Polysilicon Piezoresistors on Si(100) surface.The
polysilicon was doped with spin on dopant(phosphourous dopant) and drive
in and oxidation was done at same time at 1050C. The poly resistors are
barely 5 microns distance apart.when i measured the resistance value
the value of the resistance differed alot more than 300% change among the
adjacent resistors..

Can any one suggest me why this happened?

Thanks

kris






---------------------------------
Do you Yahoo!?
Yahoo! Web Hosting - establish your business online
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
University Wafer
Tanner EDA by Mentor Graphics