MEMSnet Home: MEMS-Talk: Etching of SiN
Etching of SiN
2003-03-13
Patrick Carlberg
Piezoresistors
2003-03-13
krishna
2003-03-17
mahdi bagheri
2003-03-18
krishna
reference material
2003-03-18
Frederick Balagot
2003-03-17
beaton@npphotonics (Bill Eaton)
2003-03-13
Hong Wu
2003-03-13
Roger Shile
2003-03-13
[email protected]
2003-03-13
Michael D Martin
2003-03-13
[email protected]
Etching of SiN
[email protected]
2003-03-13
For wet etching of silicon nitride, the standard etchant phosphoric acid,
heated to around 160 C. This is hard to mask however.

PECVD nitrides can be etch with HF solutions. I suggest 5:1 BHF for its
stability.
The etch rate will vary with the composition. I have measured 8-60 nm/min
for different PECVD recipes. BHF can be masked with photoresist.

For dry etching, both CF4 + O2 and SF6 + O2 plasmas work,
and can be patterned with photoresist (but the selectivity may not be good).

        --Kirt Williams, Ph.D.  Consultant

> -----Original Message-----
> From: Patrick Carlberg [mailto:[email protected]]
> Sent: Thursday, March 13, 2003 1:15 AM
> To: [email protected]
> Subject: [mems-talk] Etching of SiN
>
>
> Dear all,
>
> Could anyone tell me how what to use for dry and wet etching of SiN
> grown in PECVD (So there is probably some H in ther as well)
>
> Thanks
> Patrick Carlberg
> __________________________________________________
> Patrick Carlberg, Ph.D Student, MSc
> Lund University, Solid State Physics/Nanometer Consortium
> Box 118, SE-221 00 LUND, Sweden
>
> Delivery address: Sölvegatan 14, SE-223 62, LUND, Sweden
> Visiting address: Professorsgatan 1, SE-221 00, LUND, Sweden
>
> Tel:       + 46 46 222 44 95 (office)
> Fax:      + 46 46 222 36 37
> e-mail: [email protected]
> URL: http://www.ftf.lth.se/, http://www.nano.ftf.lth.se
> ___________________________________________________
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
University Wafer
Addison Engineering