Hong Wu
2003-03-14
Brent Garber
2003-03-14
Hong Wu
Cr/Si interface.
Hong Wu
2003-03-14
Thank you for the response, Brent. Yes I can do sputter Cr. The thing
worries me is the the property of Cr/Si alloy after sintering. Do you have
any idea?

Hong Wu

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Brent Garber
Sent: Thursday, March 13, 2003 7:07 PM
To: [email protected]
Subject: [mems-talk] Cr/Si interface.


Wu,

I would need to know what kind of contact you want.  Cr makes great
contact with Si when HF dipped and the Cr deposited as soon as
possible.  Being able to sputter etch the Si in the vacuum system before
deposition is best.  Are you working with bare Si?  Can you sputter Cr
instead of evaporate?

Brent
 [email protected]


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics
Nano-Master, Inc.