MEMSnet Home: MEMS-Talk: Bubbles in my SU-8
Bubbles in my SU-8
2003-03-14
frank berisford
2003-03-17
Christopher F. Blanford
2003-03-17
Jennifer Pagan
2003-03-17
Josef Kouba
2003-03-18
Mark Shaw
heat effect on MUMPS cantilever beam
2003-04-04
weiwei2
Bubbles in my SU-8
Josef Kouba
2003-03-17
It is a question of how handy you are... There are many techniques, I
would say one per user.. I usually use a small cup and pour the resist
into it first. You can remove the bubbles from the cup already, if there
are any, but I usually don't have them. Then pour the resist on the
substrate.. Using a plastic pipette (I'm using one with about 1 mm
diameter), you can again remove the bubbles, if you see some. After
spinning, you can use a blade or any other sharp object... Also, placing
the sample on well-leveled plate and heating up to around 60 deg will
remove few bubbles as the resist becomes more liquid.

Good luck!

J.

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of frank berisford
Sent: Friday, March 14, 2003 11:08 AM
To: [email protected]
Subject: [mems-talk] Bubbles in my SU-8



Hello all,

I've been trying several different techniques in an attempt to minimize
bubbles in my SU-8.  At first I tried pippeting it onto my substrate
using a large bore pippette.  I also tried dispensing from a syringe and
pouring straight from the bottle.  The pouring seems to work best but I
still get a sizable bubble count.  From here I've tried sucking the
bubbles out with a needle and syringe but to no avail.

I've read of others wiping the SU-8 across the wafers but have yet to
try this method for fear of destroying the substrate.  For what it's
worth I'm using SU-8 2035 with a target thickness of 50microns but I
think I've got my spin recipe locked down.

Thanks for  your time,
Frank Berisford




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation
Harrick Plasma, Inc.