pyrex 7740
sp
2003-03-19
Ravi,

We can produce holes in the Pyrex glass wafer. You can contact me at
[email protected]
with the details and I would be happy to help.

Thanks,
Steve Pence
408-980-9324


----- Original Message -----
From: "Ravi Shankar" 
To: 
Sent: Wednesday, March 19, 2003 4:14 AM
Subject: [mems-talk] pyrex 7740


> could anyone tell me the rough estimate of price of 6" pyrex glass wafer
> with holes drilled in them.
> Regds
> Ravi Shankar
> India
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation