MEMSnet Home: MEMS-Talk: Overlay between front and back of wafer
Overlay between front and back of wafer
2003-03-19
Mark van der Heijden
2003-03-19
Roger Brennan
2003-03-19
Luesebrink Helge
2003-03-19
Shay Kaplan
2003-03-19
Brubaker Chad
2003-03-20
Phillipe Tabada
Overlay between front and back of wafer
Phillipe Tabada
2003-03-20
Hi Mark,

   If a Carl Suss MA6 contact mask aligner is available to you, you can use
its backside alignment capabilities to measure overlay between front and
backside of the wafer.

Phil






>From: "Mark van der Heijden" 
>Reply-To: General MEMS discussion 
>To: [email protected]
>Subject: [mems-talk] Overlay between front and back of wafer
>Date: Wed, 19 Mar 2003 13:31:56 +0000
>
>
>Hi All,
>
>Does anyone know of a method/device to measure which i can use to measure
>the overlay between structures on the front and the back of a wafer.
>
>Thanks,
>Mark
>
>
>
>
>_________________________________________________________________
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/


_________________________________________________________________
Add photos to your messages with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
The Branford Group