A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Titanium etchant
Titanium etchant
2003-03-23
Yair
2003-03-25
Kirt & Erika Zipf-Williams
Titanium etchant
Yair
2003-03-23
Hi all, can anyone tell me if he'd worked with either:
NH4OH:H2O2:H2O(1:1:5)  or
H2O:H2O2:HF(20:1:1)
as etchants for Titanium? What was the etch rate, and do you know of the
selectivity over SiO2?
Thanks a lot,

Yair Gannot, Process Engineer
Wolfson Microelectronics Research Center
Dept. of Electrical Engineering
Technion, Haifa 32000, Israel
e-mail: [email protected]
tel:    972-4-8293291
fax:    972-4-8322185


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
MEMStaff Inc.
The Branford Group