Does anyone know where one can get wafer bonding services?  We are
interested in bonding silicon wafers (4 inches) using either Anodic or
Solder Glass techniques.  Any information will be appreciated.  Thanks
--
Ying Hsu
MicroSensors, Inc.
[email protected]
***********************