Dear Yair,
I normally use mixture NH4OH/H2O2 with the ratio of
1:2 or 1:3 at room temperature (both items are
concetrated) and 100 nm thick layer of Ti is removed
in about 30 - 40 seconds. It does not have any effect
on silicon oxide or silicon. Ammonia hydroxide does
atack silicon bu not with the presence of H2O2, which
suggests that the H2O2 oxidize the silicon surface and
the oxide is totaly inert.
Pavel

__________________________________________________
Do you Yahoo!?
Yahoo! Platinum - Watch CBS' NCAA March Madness, live on your desktop!
http://platinum.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
MEMS Technology Review
University Wafer