Dear Hong,

With respect to the compatibility of SU-8 to positive photoresists I can say
that as long as the SU-8 has been exposed and post-exposure baked there should
be no attack of the solvent in the PR on the cross-linked SU-8. However
depending on the solvent contained in the PR there could be some attack and even
development of the unexposed/uncrosslinked regions of the SU-8, potentially
creating a new species and causing scumming during development of the imaged
PR...

If you would like to discuss this in greater detail please do not hesitate to
contact me.

Mark Shaw
Technical Sales & Applications Support
MicroChem Corp.

email: [email protected]
url: www.microchem.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.
Addison Engineering