Dear MEMS-Colleagues,

We published a paper about an electrochemical etching technique for deep
trenches:
M. Christophersen, P. Merz, J. Quenzer, J. Carstensen , and H. Föll, Deep
electrochemical trench etching with organic hydrofluoric electrolytes, Sensors
and Actuators A, 88(3) (2001) 241-246

If you need more information, send me an email.

With best regards
    Marc


Marc Christophersen, PhD
University of Rochester
601 Elmwood Ave, Box CFH
Rochester, NY 14642
Email: [email protected]



General MEMS discussion  schrieb am 26.03.03 14:21:31:
>
> hi mems workers,
>
> can we, by any means control the side wall angle in
> etching the Si wafer with anisotropic KOH other than
> that permitted by the (111) etch stop layers?
>
> Also, can abyone let me know how we can get the
> vertical walls by etching away with KOH?
>
> Thanks and regards.
>
> Ramji Dhakal
> Binghamton, NY
>
> =====
> _________________________________________________________________Ramji Dhakal
>
> M S Mechanical Engineering,
> SUNY Binghamton, NY
>
> __________________________________________________
> Do you Yahoo!?
> Yahoo! Platinum - Watch CBS' NCAA March Madness, live on your desktop!
> http://platinum.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


____________________________________________________________________________
ImmobilienScout24 - Über 170.000 Immobilien - Finden Sie hier Ihre neue
Traumwohnung! In Immobilien die Nr.1 im Netz: http://info.is24.de/web.de


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering