Re:etching for vertical walls
2003-03-26
Rahul Agarwal
Re:etching for vertical walls
Rahul Agarwal
2003-03-26
Hello Ramji,
I don't know whether we can control the side wall angle in etching the si
anisotropically.
But regarding getting the vertical walls in a (100) silicon wafer using KOH,
the trick here is to align the rectangular/square mask opening at at angle
of 45 degrees to the crystal wafer flat which is <110>. By doing so the
{100} faces are introduced as sidewalls. the {110} planes etch faster than
the {100} planes and are not introduced as sidewalls at any point. as the
bottom and sidewalls are both from {100} gp, lateral undercut equals the
vertical etch rate and vertical walls will be produced.
Regards
Rahul agarwal
University of South Florida
Electrical Engineering Dept.
Micro Electro Mechanical Systems Lab


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.