Hi Ramji Dhakal
you can create vertical walls using Si (110) wafers etched in KOH solution.
use 44 gr per 100 ml. DI water at 80 C , use Si Nitride as a mask.
good luck,
Miriam Hershcovitz - TeraOp

-----