2003-03-21
Yinbao Yang
etching for vertical walls
2003-03-25
ramji dhakal
2003-03-27
FOCI_amou
etching for vertical walls
FOCI_amou
2003-03-27
Dear Ramji,
You can try patterning  the wafer rotated in 45 degree.

Mike Lin
Chu-Nan,Taiwan

----- Original Message -----
From: ramji dhakal 
To: General MEMS discussion 
Sent: Wednesday, March 26, 2003 5:46 AM
Subject: [mems-talk] etching for vertical walls


> hi mems workers,
>
> can we, by any means control the side wall angle in
> etching the Si wafer with anisotropic KOH other than
> that permitted by the (111) etch stop layers?
>
> Also, can abyone let me know how we can get the
> vertical walls by etching away with KOH?
>
> Thanks and regards.
>
> Ramji Dhakal
> Binghamton, NY
>
> =====
> _________________________________________________________________Ramji
Dhakal
>
> M S Mechanical Engineering,
> SUNY Binghamton, NY
>
> __________________________________________________
> Do you Yahoo!?
> Yahoo! Platinum - Watch CBS' NCAA March Madness, live on your desktop!
> http://platinum.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Mentor Graphics Corporation
Nano-Master, Inc.