Hi Hugo,
   If you pretreat both surfaces with HMDS you can get super glue to
work for about an hour in 5% TMAH.

-Mike

>>> [email protected] 03/25/03 02:28PM >>>
Hello all,

Does anyone know of, or has experience with, an epoxy that is etch
resist to TMAH?  An epoxy would be the first choice, but I am open to
other ideas like solder perhaps?

The problem is, I already have singulated die so I cant deposit a film
on the backside of the die for good eutectic or solder wetting.



Thanks,
Hugo

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
MEMStaff Inc.
University Wafer