MEMSnet Home: MEMS-Talk: Silicon Nitride Deposition(room temperature)
Silicon Nitride Deposition(room temperature)
2003-03-26
Gowtham Vangara
2003-03-28
[email protected]
2003-03-28
Neal Ricks
2003-03-31
[email protected]
Silicon Nitride Deposition(room temperature)
[email protected]
2003-03-31
We at Trion Technology in Arizona have developed a low temp Nitride process
using our ICP design coupled with a new gas distribution system for the
deposition of Nitride. Unfortunately the temperatures we are working with are
around 150 degrees C. We would be interested in working with you at the lower
temperatures so if you contact me directly at 480-968-8818 x 11 we might be able
to process some samples for you. Thanks

Bob Henderson-GM
Trion Technology
1025 S. 52nd Street
Tempe, Arizona 85281
Phone: 480-968-8818
Fax: 480-968-8896
Web site: www.triontech.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.
Addison Engineering