A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: C4F8 etchant
C4F8 etchant
2003-04-03
[email protected]
2003-04-08
Isaac Wing Tak Chan
2003-04-03
[email protected]
2003-04-04
Burkhard Volland
2003-04-04
Jason Viotty
2003-04-06
Philip Lau
C4F8 etchant
[email protected]
2003-04-03
Hi MEMS Community,

I would like to know if anyone knows of a chemical that
would etch C4F8 (octofluorocyclobutane)

During the DRIE process, C4F8 is deposited for sidewall
passivation and mask protection in the alternate deposit and
etch cycles. After the DRIE I remove the photoresist AZ4620
by putting the wafers in a Barell Asher with O2 plasma
(40mTorr, 300 Watts for 10mins) and subsequent treatment
with resist strips EKC for 10 mins at 60C and AZ300T for 10
mins at 75C.
This I believe should remove the C4F8 deposits as well.

However from our SEM pictures we find that, possibly the
unremoved C4F8 acts as a mask for further Silicon etching
(in RIE)and this mask is undercut resulting in the loss of
our structures.

I would appreciate very much if someone on the list could
get back to be with an idea of how to strip the C4F8.

Sincerely
Anupama

Anupama V. Govindarajan
Graduate Student - EE MEMS laboratory
Department of Electrical Engineering
University of Washington
Campus Box 352500, Seattle WA 98195
Phone: (206)-221-5340
email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics