kishang
2003-04-14
Has anyone had significant experience etching nitride windows on silicon using
a KOH etch? I am trying to create very thin (4200 Angstroms) Silicon Nitride
windows, but my yield goes below 50%. My KOH bath is composed of KOH pellets
and water at 80 degrees C. Are there any ways to reduce wrinkles in windows? I
currently dip my wafers in cool DI water for 10 minutes and then dry them in a
120 degree oven with my pits opening upward (i.e. window surface downward).

Any help would be great. Thanks.

-- Kishan Gupta
UC Berkeley


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
University Wafer