A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: wet-etching of polyimide
wet-etching of polyimide
2003-04-12
Shadyar Farhangfar
2003-04-14
Fariborz Nadi
Stiction tests
2003-04-14
ramji dhakal
2003-04-14
Michael D Martin
2003-04-15
Robert Dean
wet-etching of silver
2003-04-21
Helen Li
2003-04-24
Kirt & Erika Zipf-Williams
2003-04-16
Andy Scholes
2003-04-16
Conor O'Mahony
2003-04-16
[email protected]
2003-04-17
Mac Daily
wet-etching of polyimide
Andy Scholes
2003-04-16
I did some work a few months ago on wet etching polyimide as a release process
rather than for patterning.  After extensive searching we finally identified an
etch which would remove the polyimide. The results were mixed, however, and the
etch we found was very aggressive.  Careful thought must be given to the other
layers on the wafer when using the etch, so it may not suit your needs.

Although I haven't given up completely with the wet etch, a dry  etch is much
easier to control and is more production friendly. There  have been postings in
the past on dry etching which you can find in the  archives.

An alternative could be to use a photosensitive polyimide which you can pattern
and develop.  We have used PI2723 from HD Microsystems for several years and are
very happy with the results.  ( www..hdmicrosystems.com/conn/offices.html  for
contact details).

If you could give more details of the process you are running I may be able to
offer a few tips.

Andy Scholes, Ph.D.
Utvecklingsingenjör
ACREO AB
SE 164 40 Kista
Sweden

>>> [email protected] 04/12/03 03:34am >>>
Dear All,

Does anybody happen to know about the wet-etching of
polyimide? Is there any "standard" etchant to wet-etch
polyimide layers?

Appreciating any hint,
Sh.Farhangfar

__________________________________________________
Do you Yahoo!?
Yahoo! Tax Center - File online, calculators, forms, and more
http://tax.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
Addison Engineering