Dave Kharas
2003-04-16
The wrinkling you're seeing in the silicon nitride
is most likely stress. If you're depositing a 4000A
thick stoichiometric LPCVD nitride you will definitely
have a compressive stress 300MPa and up, 4000A is on
the thicker side as well. I believe Berkeley should
have a recipe for tensile low stress LPCVD SiN, which
is typically silicon rich and deposited with higher
DCS to NH3 ratio than stoichiometric nitride. I've
seen ratios ranging from 4:1 to 6:1 in literature.
Its also possible to get low stress SiN using PECVD,
but these films are less durable, they usually have
many more pinholes allowing KOH leakage, and have a
much higher etch rate in HF solutions than their LPCVD
counterparts, however if this is not a problem, they
are probably easier to deposit than LPCVD films.
good luck.

dave kharas Ph.D.
Sarcon @Sarnoff Corp.



__________________________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo
http://search.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering