MEMSnet Home: MEMS-Talk: lift-off with pmma
lift-off with pmma
2003-04-17
Lorenzo Sirigu
lift-off with pmma
Lorenzo Sirigu
2003-04-17
I'm trying to make a metal lift-off by using a pmma mask written by
e-beam lithography. Prior de metal evaporation the substrate (SiO2/Si)
and the pmma mask as well were exposed to a short RIE etching done with
CF4/H2 gases. At the end of the story the problem is that the lift-off
is pretty difficult probably due to the surface modification of the
exposed pmma. Does someone can suggest me a good solvent for this kind
of lift-off?
Thanks
Lorenzo Sirigu
-----------------------------------------------------------
Lorenzo Sirigu
Institute for Photonics and Quantum Electronics-EPFL
tel. +41-21-693 54 24
fax +41-21-693 54 80
http://imowww.epfl.ch/Nanoweb/default.htm
-----------------------------------------------------------


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.