MEMSnet Home: MEMS-Talk: KOH etching-> Low SiN stress
KOH etching-> Low SiN stress
2003-04-16
Dave Kharas
2003-04-17
Michael Pedersen
KOH etching-> Low SiN stress
Michael Pedersen
2003-04-17
I thought there was a concencus that stoichiometric LPCVD films of
silicon nitride have high tensile stress (~1GPa). Nitride films with
compressive stress are more likely deposited using PECVD.

Michael P.
The MEMS Exchange

Dave Kharas wrote:
> The wrinkling you're seeing in the silicon nitride
> is most likely stress. If you're depositing a 4000A
> thick stoichiometric LPCVD nitride you will definitely
> have a compressive stress 300MPa and up, 4000A is on
> the thicker side as well.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation