MEMSnet Home: MEMS-Talk: resist with good thermal stability
resist with good thermal stability
2003-04-17
Yilei
2003-04-17
Jessica Gomez
2003-04-17
transene
resist with good thermal stability
Jessica Gomez
2003-04-17
Hi Yilei,

Maybe AZ1518 OR AZ4620 will work for you

Jessica

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Yilei
Sent: Wednesday, April 16, 2003 9:03 PM
To: [email protected]
Subject: [mems-talk] resist with good thermal stability


Hi member,
Can anyone recommend certain resist with good thermal stability that can be
used to deposit thin film using PECVD? And more, it can be easily removed
with
selection on silicon and silicon dioxide at the same time. Thanks a lot.

Regards,
Yilei








_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review