Dear colleagues

I am working on the plastic deformation of Si and poly-Si.  Could
someone answer me the following questions?

---------------------------------------------
1.  I wonder if the heat conductivity of poly-Si is higher than that of
Si.

2.  Does grain boundary act as a heat conductive(or insulation) material
in poly-Si?

3.  Can I find some literatures on stress-strain curve of poly-Si under
high temperature?
-----------------------------------------------

Thank you.


#####################################################
E.H.YANG, Ph.D
Fujita lab., 3rd Div.,
IIS, The Univ. of Tokyo,
7-22-1 Roppongi, Minato-ku, Tokyo 106, Japan
TEL. +81-3-3402-6231(ext.2354), FAX. +81-3-3402-5078
E-mail    [email protected]
http://www.fujita3.iis.u-tokyo.ac.jp/~ehyang/yang.html
######################################################


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Nano-Master, Inc.
Mentor Graphics Corporation