B doped Silicon - Aluminum Interaction
2003-04-18
Jason Rose
B doped Silicon - Aluminum Interaction
Jason Rose
2003-04-18
Hello all,

Does anybody know if aluminum can be deposited directly onto Boron doped silicon
without impacting the piezoresistivity of the p-type silicon?

If there is interaction, what type of passivation layer should be used to
prevent it?

Thanks,
Jason

--
Jason Rose
MEMS Design Manager
 Intelligent MEMS Design, Inc.
"Your Partner in MEMS Solutions"
Tel: (613) 254-8848
Fax: (613) 230-0394
Email: [email protected]
359 Terry Fox Drive
Suite 220
Ottawa, Ontario, K2L 2E7
Canada
www.imemsdesign.com
--

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMStaff Inc.