MEMSnet Home: MEMS-Talk: thermal effect on MUMPS
thermal effect on MUMPS
2003-05-05
weiwei2
2003-05-06
Cain, Mike
2003-05-06
Johnson, Stafford
thermal effect on MUMPS
Cain, Mike
2003-05-06
Try a lower temperature epoxy.  The wafers don't see a temp greater than 115C
after the metal process.

Mike

-----Original Message-----
From: weiwei2 [mailto:[email protected]]
Sent: Monday, May 05, 2003 12:25 PM
To: General MEMS discussion
Subject: [mems-talk] thermal effect on MUMPS


i did die attach of MUMPS die onto PCB using thermal cure epoxy at 150C. it
cause extra curling of MUMPS cantilever. how to solve this? is there any
literature on this?

LEOW
Universiti Teknologi Malaysia


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing