bonding and debonding
2003-05-15
Rahul Agarwal
2003-05-16
David Nemeth
Aluminium etching
2003-05-19
Seh-Won Ahn
2003-05-19
R. Brent Garber (2 parts)
2003-05-29
Wimplinger Markus
bonding and debonding
David Nemeth
2003-05-16
I've heard of people dissolving black wax in TFE and spinning it on.  Or you
could try dissolving G-Wax in acetone and trying the same thing.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On
Behalf Of Rahul Agarwal
Sent: Thursday, May 15, 2003 2:54 PM
To: [email protected]
Subject: [mems-talk] bonding and debonding


Hello Everyone,
I am looking for a spin on material which can be used for bonding and
debonding and then again bonding like wax.  For example Silicon can be
bonded using wax, and can be easily unbonded by heating. This procedure is
repeatable. Since I can't put wax in a very very uniform matter I want some
thing which is spin on. Photoresist won't work since it can't be melted once
baked. It can only be removed but i want something which can be melted again
and again.
Rahul Agarwal
Research Assistant
Univ. of south florida, Tampa
fl-33613
Ph. 813-974-3945
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering
Mentor Graphics Corporation