MEMSnet Home: MEMS-Talk: meaning of Al/2%/Si
meaning of Al/2%/Si
2003-05-16
bobo
2003-05-16
Kirt & Erika Zipf-Williams
meaning of Al/2%/Si
Kirt & Erika Zipf-Williams
2003-05-16
That's probably Al/2%Si, which is aluminum with 2% silicon by weight.
The Si in the Al used for metallization prevents it from absorbing Si when
annealing is done to form a good electrical contact to Si.

----- Original Message -----
From: bobo 
To: 
Sent: Thursday, May 15, 2003 7:13 PM
Subject: [mems-talk] meaning of Al/2%/Si


> hi,everyone, who knows the meaning of "Al/2%/Si"? Thanks a lot.
>


----------------------------------------------------------------------------
----


> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Addison Engineering