Wafer Curvature Measurements
2003-05-21
Robert D White
2003-05-21
Neal Ricks
2003-05-22
Tun Zainal Zulkifli
2003-05-26
Erhan Ata
2003-05-21
Philip D. Floyd
Wafer Curvature Measurements
Philip D. Floyd
2003-05-21
Robert,

As I remember Michigan has a great MEMS program.  Why not talk to those
guys?  A little cooperation between departments might not hurt?

Solid State Electronics Lab  http://www.eecs.umich.edu/ssel/index.php


************************************
Philip D. Floyd, Ph.D.
Iridigm Display Corporation
2415 Third Street, Suite 235
San Francisco, CA 94107
ph:  (415) 626-8800 x138
fax: (415) 626-9775
email: [email protected]
web:  http://www.iridigm.com/
*************************************
############################################################################
##############################################
This email communication may contain CONFIDENTIAL INFORMATION of IRIDIGM
DISPLAY CORPORATION and is intended only for the use of the intended
recipients identified above. If you are not the intended recipient of this
communication, you must not use, disclose, distribute, copy or print this
email. If you have received this communication in error, please immediately
notify the sender by reply email, delete the communication and destroy all
copies.
############################################################################
##############################################


-----Original Message-----
From: Robert D White [mailto:[email protected]]
Sent: Wednesday, May 21, 2003 7:14 AM
To: [email protected]
Subject: [mems-talk] Wafer Curvature Measurements

I am looking for someone to do some pre- and post- wafer curvature
measurements for estimation of residual stresses evolved during LPCVD
deposition.  I would be doing the LPCVD step myself, and want to send
the wafers somewhere to get the measurements done before and after.
Does anyone offer this service or know where I might look?

Many thanks,

Rob
--
Robert D. White
Graduate Student Research Assistant
Vibrations and Acoustics Lab, 2200 EECS
Mechanical Engineering
University of Michigan
Ann Arbor, MI 48109

(734)936-3824
[email protected]

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing