MEMSnet Home: MEMS-Talk: Oxidation after DRIE
Oxidation after DRIE
2003-06-06
BenoîtGAULIER
2003-06-09
Lawlor, Chris
2003-06-09
Justin Borski
Oxidation after DRIE
Lawlor, Chris
2003-06-09
Dear Benoit,

We, at Analog Devices in Belfast, would be happy to assist, we are a
manufacturer of SOI substrates.
One of our core products, the BCO substrate, is based on DRIE of SOI with
additional oxide processes to create dielectrically isolated features.
Please feel free to contact me for further discussions,

With regards,
Chris.


-----Original Message-----
From: Benoît GAULIER [mailto:[email protected]]
Sent: 06 June 2003 15:36
To: General MEMS discussion
Subject: [mems-talk] Oxidation after DRIE


Dear Colleagues,

Am searching for practical information / experience on thermal oxidation after
DRIE Bosch process. I'm using SOI wafers and i want to oxide the wafers after
the DRIE step Does anybody know if this process is possible? Any experiences,
information, recipes, etc would be greatly appreciated.

Best regards,

Benoît GAULIER.

=================================================
   Benoît GAULIER
   Ingénieur Filière Microtechnologie
   THALES AVIONICS
   NAVIGATION
   25, rue Jules Védrines 26027 Valence CEDEX
   Télécopie: (+33) (0) 4-75-79-86-06
   Bureau: (+33) (0) 4-75-79-88-25
=================================================



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list options,
visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at
http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMStaff Inc.