PECVD n-type a-Si:H
2003-06-12
Jobert van Eisden
2003-06-20
Hong Wu
PECVD n-type a-Si:H
Hong Wu
2003-06-20
Call Dick at Scientific Coating. http://www.wso.net/scl/

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Jobert van Eisden
Sent: Thursday, June 12, 2003 7:53 AM
To: '[email protected]'
Subject: [mems-talk] PECVD n-type a-Si:H


Dear all,

I am looking for an outside source for depositing up to 8000 Angstroms
of PECVD n-type hydrogenated amorphous silicon, with various gas phase
Phos. doping concentrations. The depositions would have to be done on small
to medium size lots of 8" wafers, and if to our likings, future lots up to
50 wafers a month. The maximum temperature for the deposition is 340 deg.C.
If you can, or know somebody who can do this, please let me know and yes,
qoutes are welcome.

Regards,

Jobert van Eisden
[email protected]
UAlbany Institute for Materials
SUNY Albany

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing