Dlee Li
2003-06-23
Roger Shile
2003-06-23
Jobert van Eisden
PECVD Si3N4 recipe
Jobert van Eisden
2003-06-23
Look on th CNF website
http://www.cnf.cornell.edu/cnfprocesses/cnf_process.htm
They have a recipe I've beem using for a parallel plate PECVD tool.

Jobert van Eisden

SUNY Albany

-----Original Message-----
From: Dlee Li
To: [email protected]
Sent: 6/20/2003 5:17 PM
Subject: [mems-talk] PECVD Si3N4 recipe

Hi,
anyone can give me his workable PECVD Si3N4 recipe? we need to add PECVD

Si3N4 to our system.

thanks
Dlee

_________________________________________________________________
MSN 8 helps eliminate e-mail viruses. Get 2 months FREE*.
http://join.msn.com/?page=features/virus


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Addison Engineering
Tanner EDA by Mentor Graphics