Platinum electroplating
2003-06-24
sokwon Paik
Platinum electroplating
sokwon Paik
2003-06-24
My name is sokwon Paik and I'm a Ph.D student of Texas
A&M University.
I want to electroplate platinum on my wafer on top of
gold.
Anybody knows the vendor and recipe for the platinum
electroplating?
Please let me know if you have any idea about this.

Thanks,


Sokwon Paik

__________________________________
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
http://sbc.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics
Nano-Master, Inc.