A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Anodic Bonding
Anodic Bonding
2003-06-17
mems greenhorn
2003-06-24
Tony Rogers
laser Machining
2003-06-26
Shay Kaplan
2003-06-26
Mark da Silva (2 parts)
2003-06-26
Mario Robles
2003-06-23
Tomblin, Graham (OH32)
Anodic Bonding
Tony Rogers
2003-06-24
Have a look at the following:

T. Rogers and J. Kowal.

"Selection of glass, anodic bonding conditions and material compatibility
for silicon/glass capacitive sensors"

Published in Eurosensors VIII, 1994.

Sensors and Actuators A 46-47 (1995) 113-120

Regards

Tony

Tony Rogers
Applied Microengineering Ltd
173 Curie Avenue
Didcot
OX11 0QG
UK
Tel.: +44 (0)1235 833934
Fax: +44 (0)1235 833935
e-mail: [email protected]

Web:http://www.aml.co.uk


-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of mems greenhorn
Sent: 18 June 2003 00:34
To: [email protected]
Subject: [mems-talk] Anodic Bonding


Can anyone let me know where I can find a good paper on Anodic
Bonding..Trying to do the anodic bonding at device level for the first
time..so need info on the procedure involved ...
- Are there any restrictions on the type of  Oxidation ( Thermal or PECVD)
that Si wafer should have..
- What wafer thickness and oxide thickness would be ideal. ?
- What voltage and temperatures ?
- Significance of the mechanical pressure...?
- Is vaccum a must ?
Any other info that u can give to get a good bonding would be of great help
!
Thanks in advance.
MEMS_GREENHORN


---------------------------------
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering