We are working on a dry gold plasma etch process right now. It is not ion beam
etching but I am not at liberty to discuss in open forum right now. You can
contact me directly at 480-968-8818 x 11 at Trion Technology and I will see if
this is an appropriate application for you. Must be thin gold layer <2000
angstroms. Bob Henderson