MEMSnet Home: MEMS-Talk: Cu Metal Etchant
Cu Metal Etchant
2003-07-02
이태원
2003-07-02
Greg Reimann
Making holes in Pyrex glass wafers?
2003-07-03
Gautham Viswanadam
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-07
Bill Flounders
2003-07-09
Carsten Wesselkamp
2003-07-03
David Nemeth
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-02
Pavel Neuzil
2003-07-03
Lin, Yaojian
Cu Metal Etchant
David Nemeth
2003-07-03
Ferric Chloride in water will etch copper.  It's used to make printed
circuit boards.
I strongly suspect an adhesion layer would be necessary for copper on
silicon, but I have no direct experience.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of 이태원
Sent: Wednesday, July 02, 2003 11:01 AM
To: [email protected]
Subject: [mems-talk] Cu Metal Etchant


hi.

I heard about Cu could be patterned by something like CMP Process
 damascene(?) process)

Are there any wet etchants fot Cu etch? If not, what is the main reason
about that?

Furthermore, Adhesion layer (Ti or Cr) is not required when I deposit Cu on
Si Wafer ?

Thank you for in Advance.

TW Lee.

-----------------------------------------------------------
AeroMEMS Laboratory.
School of Mechanical & Aerospace Engineering.
Seoul National University , Seoul , KOREA.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review
Harrick Plasma, Inc.