Hello,

I'm working on an optical sensor integrated on silicon with phase
modulation driven by acoutic surface waves (ZnO piezoelectric thin
film)on the reference arm.
The architecture of this sensor is a Mach-Zehnder interferometer and in
order to isolate the measurement arm, I need an acoustic absorber. Until
now, I just realised an isolation trench by deep RIE etching.

Could someone help me ?

Thanks


--
Dr. Eric Bonnotte
LIMMS/Kawakatsu laboratory / CNRS/IIS-The University of Tokyo
7-22-1 Roppongi Minato-ku Tokyo 106 JAPAN
Tel/FAX : +81-3-3402-9568
Tel/Fax Home : +81-3-3411-5381
E-mail : [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
MEMStaff Inc.