MEMSnet Home: MEMS-Talk: LAM etcher troubles
LAM etcher troubles
2003-08-01
Luckett, James T
2003-08-01
Alan D. Raisanen
2003-08-01
[email protected]
LAM etcher troubles
[email protected]
2003-08-01
You noted the main physical differences in the 490 vs. 590. Lam used the 590
primarily for oxide/nitride etches using CF4 and other gases. The 490 was used
for etching using chlorine processes such as for polysilicon. They are both top
powered and the graphite on the 590 can tend to generate particles through time
and needs to be replaced as a consumable. No such problem with the anodized
version on the 490. In my opinion the 490 was a great polysilicon etch tool but
the 590 was a marginal oxide etcher. I think Tegal made a better oxide etcher in
the Tegal 903e. Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group
Harrick Plasma, Inc.