Glass-Glass bonding
Mark Fuller
2003-08-05
At 04:45 PM 8/4/2003 -0500, you wrote:
>Hello all,
>  I am interested in bonding two glass wafers (one can be pyrex) together.
 prior to bonding i etch a microchannel into of the substrates using BOE.
Does anyone know of materials that can be used as a masking material for
BOE etching and as an intermediate layer for bonding?I know that aluminium
can be used as a intermediate layer for bonding but it does not hold up to
the BOE etching. I am also will to try gold-gold thermocompression bonding
but am not familar with the process so if someone also has information on
this bonding method it will be greatly appreciated.
>
>Thank you.
>Ryan
>

Well you could do your BOE etch of the glass.  Most standard photoresists
should stand up to that.  Then sputter aluminum on, pattern and etch that
with an aluminum etchant to expose your channels, and then do your bond.

--
Mark Fuller
Microelectronics Fabrication Facility
Washington State University
Dana Hall 102
Pullman, WA  99164-2711
(509)335-1797

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation